Table of Contents

PVC Extrusion: Twin-screw Extruder Parameters and Configuration

A twin-screw extruder is a critical piece of equipment in PVC extrusion. PVC extrusion involves melting and shaping PVC resin into finished products such as pipes, sheets, and films. Different types of twin-screw extruders and screw designs are suited for rigid and flexible PVC products, ensuring efficient processing while minimizing material degradation and energy consumption.

Choosing the Type of Twin-Screw Extruder for Different PVC Products

Rigid PVC products typically do not contain plasticizers and are characterized by good flexibility, easy molding, and resistance to brittleness. They are widely used in pipes, sheets, and plates. They are widely used in pipes, sheets, plates, etc.

For rigid PVC products, a conical twin-screw extruder is recommended. Conical twin-screw extruders have smaller screw channel volumes and enhanced extrusion effects, providing higher energy conversion for better pre-plasticization. These extruders feature larger feeding section diameters, which help with heat transfer and shearing of the material, improving the plasticization effect. Additionally, the conical design helps avoid excessive frictional heat during extrusion, reducing the risk of material degradation.

Flexible PVC products typically contain plasticizers and are mainly used in cables, hoses, films, etc.  

For soft PVC products, a co-rotating twin-screw extruder is recommended. Co-rotating twin-screw extruders offer high mixing efficiency, making them suitable for material blending, modification, coloring, homogenization, and low-temperature extrusion. These extruders better disperse additives and stabilizers. Since flexible PVC is sensitive to overheating, an extruder with a precise temperature control system should be selected.

Choosing the Right Twin-Screw Extruder Screw Design

1. Screw Design Principles:

PVC is a heat-sensitive material that is easy to decompose, so the screw design needs to be as low shear as possible to prevent overheating and material degradation.

The screw and barrel need to have anti-corrosion properties to extend the service life of the equipment.

2. Screw Parameters:

Length-to-diameter ratio (L/D): It is recommended to select L/D=20~40, which can provide sufficient compression and plasticizing effects while avoiding excessive shearing.

Compression ratio (ε): The compression ratio of PVC is generally selected between 1.6 and 2, which can ensure uniform plasticization of the material while reducing energy consumption.

Screw Tip Design: For flexible PVC products, a conical twin-screw extruder with a tip angle of 20°–30° is recommended. This design helps improve energy conversion efficiency, reduce shear heat, and meet the plasticization requirements for PVC.  

Screw Structure: PVC processing typically uses a gradient screw, which gradually transitions through the conveying, heating, compression, and venting sections, helping improve mixing efficiency and uniformity in plasticization.

Other Considerations:

The screw surface needs to be chrome-plated to improve wear resistance and corrosion resistance.

During the production process, the screw parameters, such as compression ratio, aspect ratio, etc., should be adjusted according to the actual product requirements to achieve the best plasticization effect.

Set the Appropriate Temperature

Feed Section (hopper area):

The temperature of the feed section is usually lower to prevent the material from agglomerating at the feed port. It is generally recommended to set the temperature at around 40-90℃.

This ensures that the PVC resin does not stick or block the feed port while allowing air to escape effectively. The feed section temperature should be higher than the melting temperature of the PVC resin to avoid poor plasticization caused by the material staying in the feed section for too long.

Melting Section (compression section):

The PVC begins to transition from a glassy state to a viscous flow at around 160°C, with gelation starting at 150°C. The melting section should have a linear temperature increase to facilitate proper fusion and plasticization.

Homogenizing Section (metering section):

The temperature of the homogenizing section can be controlled between 170℃-180℃ to ensure the uniformity of the material and prevent overheating.

Mold Outlet (final melt temperature):

The temperature of the mold outlet is usually higher, generally set between 190℃-210℃ to ensure that the melt can pass through the mold smoothly and form the desired shape.

Social Media:

Facebook
Twitter
LinkedIn
Pinterest

Social Media

Contact Us

Related Posts

Inquiry Form

Fill out the form below to contact us, and you'll receive a reply from us within 12 hours.

Inquiry Form

Fill out the form below to contact us, and you'll receive a reply from us within 12 hours.

Descargar PDF

Complete el formulario para obtener nuestro catálogo más reciente

Formulario de Consulta

Complete el formulario a continuación para contactarnos y recibirá una respuesta en un plazo de 12 horas.

Download PDF

Fill Out The Form To Get Our Latest Catalog

Download PDF

Fill Out The Form To Get Our Latest Catalog